What is the definition of superalloy?

  • An alloy consisting of three or more elements that is very expensive and designed to perform at elevated temperatures.
  • Learn more about superalloy in the class "Nonferrous Metals and Alloys 220" below.

Nonferrous Metals and Alloys 220

Materials Training


Class Information
ToolingU.com classes are offered at the beginner, intermediate, and advanced levels. The typical class consists of 12 to 25 lessons and will take approximately one hour to complete.
Class Name:Nonferrous Metals and Alloys 220
Description:This class identifies the major categories, properties, and uses of nonferrous metals and their alloys.
Prerequisites: 500120 
Difficulty:Intermediate
Number of Lessons:14
Language:English, Spanish
  

Below are all the competencies and job programs that contain the class Nonferrous Metals and Alloys 220. Job programs are our traditional class lists organized according to common job functions. Competencies are our latest job-specific curricula that help tie online learning to practical, hands-on tasks.

Click on any title to view its details.


Class Outline
  • Objectives
  • Nonferrous Metals Today
  • Definition of an Alloy
  • Properties of Aluminum
  • Aluminum Alloys
  • Properties of Copper
  • Copper Alloys
  • Titanium Alloys
  • Magnesium Alloys
  • Nickel and Zinc Alloys
  • Lead and Tin
  • Superalloys
  • Selecting the Best Alloy
  • Summary
  
Class Objectives
  • Describe nonferrous metals.
  • Define alloy.
  • List the properties of aluminum.
  • Describe the properties of aluminum alloys.
  • Describe common uses of copper.
  • Identify the main ingredients of copper alloys.
  • Describe the properties of titanium alloys.
  • Describe the properties of magnesium alloys.
  • Identify uses for nickel and zinc alloys.
  • Describe the properties of lead and tin.
  • Define superalloy.
  • Describe how to select the best alloy.

Class Vocabulary  
alloy     A metal consisting of two or more materials. One of these materials must be a metal.
aluminum     A silvery white metal that is soft, light, and has a high strength-to-weight ratio.
brass     An alloy of copper and zinc. Brass offers a balance of electrical and thermal conductivity and strength.
bronze     An alloy of copper and tin. Bronze offers a balance of strength, wear resistance, and corrosion resistance.
cobalt     A shiny, grayish metal that is brittle and hard, with magnetic properties similar to iron.
coefficient of thermal expansion     The change in density that occurs as a material changes in temperature. A metal typically increases in volume and decreases in density as it is heated.
copper     A reddish metal that is very ductile, thermally and electrically conductive, and corrosive resistant. Copper is often used to make electrical wire.
corrosion resistance     The ability of a metal to withstand the deterioration and chemical breakdown that occurs during surface exposure to a particular environment.
creep strength     The ability of a metal to withstand a constant weight or force at elevated temperatures.
die casting     A metal casting that is made by injecting the molten metal into a cavity under pressure.
ductility     The ability of a metal to be drawn, stretched, or formed without breaking.
electrical conductivity     The ability of a metal to convey an electric current.
ferrous metal     A metal in which iron is the main ingredient.
galvanized steel     Steel that has been plated with zinc to improve corrosion resistance.
heat treatment     The controlled heating and cooling processes used to change the structure of a material and alter its physical and mechanical properties.
hexagonal close-packed     The crystal structure that contains a collection of atoms that are closely packed into the shape of a hexagon. Metals with a hexagonal close-packed crystal structure are very difficult to form.
lead     A bluish white metal that is very soft and ductile and is a poor conductor of electricity. Lead is used as a soldering alloy and as a sound dampener.
magnesium     A grayish white, extremely light metal that is also brittle and has poor wear resistance.
modulus of elasticity     A variable that describes the relationship of stress to strain within the material's elastic region. It describes the stiffness of a material.
nickel     A silvery white metal that is fairly hard and malleable, with properties similar to iron and steel. Nickel is used as a plating metal for steel.
nonferrous metal     A metal that does not contain iron as a main ingredient.
ore     The impure, natural state of a metal.
oxide coating     A protective film that develops on the surface of a metal.
plain carbon steel     The basic type of steel, which contains less than 3% of elements other than iron and carbon.
plating metal     A metal that is added as a protective coating for another metal.
soldering alloy     A metal alloy that is melted at relatively low temperatures and used to join metal parts.
strength-to-weight ratio     The relationship between a material's strength and its weight. Materials that are light but also very strong have a high strength-to-weight ratio.
superalloy     An alloy consisting of three or more elements that is very expensive and designed to perform at elevated temperatures.
thermal conductivity     The ability of a material to conduct heat.
tin     A silvery white metal that is very soft and has poor strength. Tin is used in soldering alloys.
titanium     A silvery white metal that has a high strength-to-weight ratio and is corrosive resistant. Titanium is often used in aerospace applications.
zinc     A bluish white metal that is corrosive resistant and has a relatively low melting point. Zinc is used as a plating metal for steel.

 





Sitemap   |   Terms of Use   |   Privacy   |   Meetings

ToolingU.com
3615 Superior Avenue East
Building 44, 6th Floor
Cleveland, OH 44114
Toll Free: +1 (866) 706-8665

© Copyright 2012 Tooling University, LLC. All rights reserved.